Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 651 °C | 1200 °F | |
MarkeTech Sodium Iodide:Thallium (Nal:Tl) Scintillator Crystal Sodium iodide activated by thallium has long been the scintillation standard. Nal:Tl has good performance, economical price, high luminescence efficiency, very good spectroscopic performance and no .. |
|||
Melting Point | 650 - 710 °C | 1200 - 1310 °F | |
Johnson Matthey Matti-sil 40Sn Cadmium Free Brazing Alloy A general purpose alloy, often used for refrigeration work.Optimum Joint Gap 0.075 - 0.2 mm.AWS A5.8-92 BAg-28BS EN 1044 1999 AG105Equivalent to Engelhard Silvaloy A-40TEquivalent to Handy & Harman .. |
|||
Melting Point | 649 - 721 °C | 1200 - 1330 °F | |
Lucas-Milhaupt BRAZE 380 Characteristics:Braze 380 is a free-flowing, low temperature filler metal with excellent wetting of most ferrous and non-ferrous base metals, and is a good substitute for cadmium-bearing filler meta.. |
|||
Melting Point | 649 - 721 °C | 1200 - 1330 °F | |
Lucas-Milhaupt Silvacore® A38T Flux Cored Brazing Alloy Silvaloy A38T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult to wet metals.. |
|||
Melting Point | 649 - 721 °C | 1200 - 1330 °F | |
Lucas-Milhaupt Silvaloy® A38T Brazing Alloy Silvaloy A38T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult to wet metals.. |
|||
Melting Point | 649 - 710 °C | 1200 - 1310 °F | |
Lucas-Milhaupt Silvaloy® A40T Brazing Alloy Silvaloy A40T is a good general purpose, low melting, cadmium-free alloy, often selected for its low temperature, wetting and good flow. Silvaloy A40T has a lower brazing temperature with a relative.. |
|||
Melting Point | 649 - 700.0 °C | 1200 - 1292 °F | |
Lucas-Milhaupt Silvacap 35490 Brazing Alloy Silvacap is a low brazing temperature, cadmium-free alloy. It has a slight plastic range which may be noticed during melting on some applications. Generally, the joint strength using Silvacap will s.. |
|||
Melting Point | 650 °C | 1200 °F | |
American Elements Magnesium Nanoparticles General DescriptionMagnesium (Mg) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Magnesium Particles are typically 20-60 nanometers (nm) with specif.. |
|||
Melting Point | 649 - 710 °C | 1200 - 1310 °F | |
Lucas-Milhaupt BRAZE 402 Silver Based Cadmium Free Filler Metal Characteristics: Braze 402 is a free-flowing, intermediate temperature filler metal and as such is a good substitute for cadmium-bearing filler metals with similar silver contents. The material is .. |