Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 640.0 - 681.1 °C | 1184 - 1258 °F | |
Lucas-Milhaupt BRAZE 452 Characteristics:Braze 452 is a free-flowing, low temperature filler metal commonly used to replace cadmium-bearing filler metals of similar silver content. This alloy is best suited for narrow gap .. |