Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 635.0 °C | 1175 °F | |
Heatbath/Park Sta-Hard 17 High Speed Hardening Salt A neutral salt for hardening, annealing, normalizing, or preheating high speed tools. It is non-decarburizing, making it suitable for heating alloy tool steels which require high hardening temperatu.. |
|||
Melting Point | 635.0 °C | 1175 °F | |
Heatbath/Park Sta-Hard 17 Neutral Salt A neutral salt for hardening, annealing, normalizing, or preheating high speed tools. It is non-decarburizing, making it suitable for heating alloy tool steels which require high hardening temperatu.. |