Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 567 - 903 °C | 1050 - 1660 °F | |
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Melting Point | 566 °C | 1050 °F | |
Heatbath/Park Wire Annealing Quenching and Tempering Salt Chloride and carbonate mixture recommended. For annealing nonferrous materials or for heat treating steel where slight decarburization is not desirable. Wire Annealing Salt is extremely fluid, compl.. |
|||
Melting Point | 566 °C | 1050 °F | |
Heatbath/Park Pen Kase 5 Carburizer Cyanide Liquid Carburizer. Water-soluble liquid carburizing salt offering easy cleaning, good fluidity and high stability. Will produce carbonitrided cases in lower temperature ranges and carbon c.. |
|||
Melting Point | 566 °C | 1050 °F | |
Heatbath/Park Wire Annealing Salt Neutral Salt Chloride and carbonate mixture recommended. For annealing nonferrous materials or for heat treating steel where slight decarburization is not desirable. Wire Annealing Salt is extremely fluid, compl.. |
|||
Melting Point | 565 - 572 °C | 1050 - 1060 °F | in contact with aluminium |
Solvay Chemicals NOCOLOK® CB Flux Potassium Silicofluoride Reactive flux for brazing of aluminumCAS-No.: 16871-90-2 Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical AppliancesInformation provided .. |
|||
Melting Point | 565 - 572 °C | 1050 - 1060 °F | |
Solvay Chemicals NOCOLOK® Flux Drystatic Potassium Fluoroaluminate Flux using electrostatic/dry powder coating. Classifications: HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & .. |
|||
Melting Point | 565 - 572 °C | 1050 - 1060 °F | |
Solvay Chemicals NOCOLOK® Flux P2 Potassium Fluoroaluminate Mixtures of NOCOLOK® Flux P2 with NOCOLOK® Flux allow for gradual viscosity adjustments in suspensions to suit specific process conditions.HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automoti.. |
|||
Melting Point | 564 - 572 °C | 1050 - 1060 °F | |
Solvay Chemicals NOCOLOK® Flux Potassium Fluoroaluminate A high quality fluxing agent for brazing aluminum components. Classifications: HS No.: 38109090/CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration .. |
|||
Melting Point | 564 - 572 °C | 1050 - 1060 °F | NOCOLOK Flux |
Solvay Chemicals NOCOLOK® Sil Flux (fine grade) Reactive flux for brazing of aluminum and filler alloy generating flux for brazing aluminum. Classifications: HS No.: 38109090 /CAS-No.: 60304-36-1Composition: either 2:1: 66.6 % ± 1.5 % -NOCOLOK.. |
|||
Melting Point | 565 - 572 °C | 1050 - 1060 °F | (Addition of CsAIF4 will reduce melting point) |
Solvay Chemicals NOCOLOK® Ultra Flux Paste A flux paste specifically formulated for providing a viscous homogeneous mixture of NOCOLOK® Flux (35–50%) in an organic carrier for brazing aluminum cladded interfaces where traditional wat.. |
|||
Melting Point | 565 - 575 °C | 1050 - 1070 °F | in contact with Al/Si filter metal |
Solvay Chemicals NOCOLOK® Zn Flux Reactive flux alternative to arc spray Zn coating.HS No.: 38109090 /CAS-No.: 13827-02-6Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical .. |
|||
Melting Point | 564 - 572 °C | 1050 - 1060 °F | NOCOLOK Flux |
Solvay Chemicals NOCOLOK® Sil Flux (extra fine grade) Reactive flux for brazing of aluminum and filler alloy generating flux for brazing aluminum Classifications: HS No.: 38109090 /CAS-No.: 60304-36-1Composition: either 2:1: 66.6 % ± 1.5 % -NOCOLOK .. |