Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 38.0 - 43.0 °C | 100 - 109 °F | |
Indium Corp. Indalloy 15 Low Melting Bismuth Alloy Information Provided by Indium Corporation |
|||
Melting Point | 37.9 °C | 100 °F | |
LG Chemical Phenol Structure & Characteristics: C6H5OH. Phenol is a white crystalline solid with a distinct smellUses: Raw material of phenolic resins, dye stuffs, synthetic fibers, herbicides, photo material, aromati.. |
|||
Melting Point | 38.0 - 48.0 °C | 100 - 118 °F | |
Solvay RHODAPHOSE® DIPHENYL PHOSPHATE DIHYDRATE Phosphorus Derivative Identification: DIPHENYL PHOSPHATE DIHYDRATECAS: 838 – 85 – 7EC: 212 – 657 – 2Available in: Asia Pacific, Europe, Latin America and North America Solubility: Organic Solvents. So.. |
|||
Melting Point | >= 38.0 °C | >= 100 °F | |
BorsodChem ONGRONAT HS-44 MDI Isocyanate Monomeric 4,4`-diphenyl-methane-diisocyanate (pure-MDI).Field of application: With suitable polyols it can be used as isocyanate component for producing elastomers, adhesives, coatings, fibers, flex.. |