Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | -64.0 °C | -83.2 °F | Freezing Point |
LG Chemical Butyl Acrylate Features: Low Color - Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Through the multistag.. |
|||
Melting Point | -64.0 °C | -83.2 °F | Freezing Point |
BASF Butyl Acrylate Formula: C7H12O2CAS: 141-32-2Description: Acrylic acid ester, for manufacturing polymers and for use as a feedstock for syntheses.Applications: Butyl acrylate forms homopolymers and copolymers. Copo.. |