Polymer Property : Melting Point = 95.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 90.0 - 95.0 °C
194 - 203 °F
MQSA 70 A
Lubrizol Advanced Materials Pearlbond® D1160 Thermoplastic Polyurethane
Pearlbondâ„¢ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbo..
Melting Point 85.0 - 95.0 °C
185 - 203 °F
DSC
EMS-Griltech Griltex® D 1500A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 85.0 - 95.0 °C
185 - 203 °F
DSC
EMS-Griltech Griltex® D 1500A Copolyamide Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 85.0 - 95.0 °C
185 - 203 °F
DSC
EMS-Griltech Griltex® D 1516A Heat Stabilized Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 85.0 - 95.0 °C
185 - 203 °F
DSC
EMS-Griltech Griltex® D 1516A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications)
GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides for excellent r..
Melting Point 85.0 - 95.0 °C
185 - 203 °F
DSC
EMS-Griltech Griltex® D 1616E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 64.0 - 95.0 °C
147 - 203 °F
Average value: 78.8 °C Grade Count:8
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu..