Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 824 - 853 °C | 1520 - 1570 °F | |
Williams Advanced Alloys Wambraze™ WB853 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |