Polymer Property : Melting Point = 750 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 645 - 750 °C
1190 - 1380 °F
Johnson Matthey Matti-phos 6 Alloy for Fluxless Brazing of Copper
This alloy is a low melting point free flowing product. Joints are not as ductile as Matti-Phos 15 or Matti-phos 5.Optimum Joint Gap 0.05 - 0.2 mm.AWS A5.8-92 BCuP-4Federal Specification QQ-B-650 B..