Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 605 - 710 °C | 1120 - 1310 °F | |
Indium Corp. Indalloy 212 Ag-Cu-Zn-Cd Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 670 - 710 °C | 1240 - 1310 °F | |
Johnson Matthey Argo-braze 49LM Silver Brazing Alloy for Tungsten Carbide Brazing This material is supplied as Trifoil. Trifoil consists of a layer of copper sandwiched by brazing alloy. The copper helps to absorb the stresses caused by the differential expansion rates, under he.. |
|||
Melting Point | 650 - 710 °C | 1200 - 1310 °F | |
Johnson Matthey Matti-sil 40Sn Cadmium Free Brazing Alloy A general purpose alloy, often used for refrigeration work.Optimum Joint Gap 0.075 - 0.2 mm.AWS A5.8-92 BAg-28BS EN 1044 1999 AG105Equivalent to Engelhard Silvaloy A-40TEquivalent to Handy & Harman .. |
|||
Melting Point | 607.2 - 710 °C | 1125 - 1310 °F | |
Lucas-Milhaupt Silvaloy® 30 Brazing Alloy Silvaloy 30 is historically a modification of Silvaloy 35 with further reduction in silver content resulting in a higher melting point and a longer range. Silvaloy 30 is used for brazing steel, stai.. |
|||
Melting Point | 649 - 710 °C | 1200 - 1310 °F | |
Lucas-Milhaupt Silvaloy® A40T Brazing Alloy Silvaloy A40T is a good general purpose, low melting, cadmium-free alloy, often selected for its low temperature, wetting and good flow. Silvaloy A40T has a lower brazing temperature with a relative.. |
|||
Melting Point | 607.2 - 710 °C | 1125 - 1310 °F | |
Lucas-Milhaupt EASY FLO 30 Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo 30 is a are good general purpose, low temperature silver brazing filler metals for joining both ferrous and nonferrous metals. Because of their fairly low cost, good fatigue .. |
|||
Melting Point | 649 - 710 °C | 1200 - 1310 °F | |
Lucas-Milhaupt BRAZE 402 Silver Based Cadmium Free Filler Metal Characteristics: Braze 402 is a free-flowing, intermediate temperature filler metal and as such is a good substitute for cadmium-bearing filler metals with similar silver contents. The material is .. |