Thermal Properties Metric English Comments
Melting Point 603 - 705 °C
1120 - 1300 °F
Indium Corp. Indalloy 179 Silver Solder Alloy
Information Provided by Indium Corporation
Melting Point 680 - 705 °C
1260 - 1300 °F
Johnson Matthey Argo-braze 49H Silver Brazing Alloy for Tungsten Carbide Brazing
Optimum Joint Gap 0.1 - 0.25 mm.AWS A5.8-92 BAg-22BS EN 1044 1999 AG502Equivalent to Engelhard Silvaloy A-49NMEquivalent to Handy & Harman Braze 495Information provided by Johnson Matthey.
Melting Point 660 - 705 °C
1220 - 1300 °F
Johnson Matthey Argo-braze 502 Silver Brazing Alloy for Tungsten Carbide Brazing
These products are specifically designed for brazing of tungsten carbide tips to steel tools and wear parts. Optimum Joint Gap 0.1 - 0.25 mm.AMS 4788AWS A5.8-92 BAg-24Equivalent to Engelhard Silvalo..
Melting Point 640 - 705 °C
1180 - 1300 °F
Indium Corp. Indalloy 211 Ag-Cu Solder Alloy
Information Provided by Indium Corporation
Melting Point 630 - 705 °C
1170 - 1300 °F
Williams Advanced Alloys Wambraze™ WB705 Solder
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de..