Thermal Properties Metric English Comments
Melting Point 649 - 700.0 °C
1200 - 1292 °F
Lucas-Milhaupt Silvacap 35490 Brazing Alloy
Silvacap is a low brazing temperature, cadmium-free alloy. It has a slight plastic range which may be noticed during melting on some applications. Generally, the joint strength using Silvacap will s..