Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 57.0 - 67.0 °C | 135 - 153 °F | |
Fine Organics FINALUX G 120 Lubricant Additive Applications: Lubricant for rigid PVC fittings, films and other Sn-mercaptide stabilized articles. Suitable for PVC cable compounds.Information provided by Fine Organics |
|||
Melting Point | 63.0 - 67.0 °C | 145 - 153 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 121 Linear Thermoplastic Polyurethane Pearlbond™ 121 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit.. |
|||
Melting Point | 63.0 - 67.0 °C | 145 - 153 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 101 Linear Thermoplastic Polyurethane Pearlbond™ 101 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity leve.. |
|||
Melting Point | 63.0 - 67.0 °C | 145 - 153 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 501 Linear Thermoplastic Polyurethane Pearlbond™ 501 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a high crystallization rate and a very high thermoplasticity level.Appli.. |
|||
Melting Point | 63.0 - 67.0 °C | 145 - 153 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 521 Linear Thermoplastic Polyurethane Pearlbond™ 521 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.Appl.. |