Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 60.0 - 64.0 °C | 140 - 147 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 523 Linear Thermoplastic Polyurethane Pearlbond™ 523 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level... |
|||
Melting Point | 60.0 - 64.0 °C | 140 - 147 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 123 Linear Thermoplastic Polyurethane Pearlbond™ 123 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit.. |
|||
Melting Point | 60.0 - 64.0 °C | 140 - 147 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 503 Linear Thermoplastic Polyurethane Pearlbond™ 503 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a high crystallization rate and a very high thermoplasticity level.Appli.. |
|||
Melting Point | 61.0 - 64.0 °C | 142 - 147 °F | Fisher Johns |
Solvay MACKAMIDE® CMA Surfactant Product Description: Mackamide CMA is a 1:1 coconut monoethanolamide, which is designed for use in household and cosmetic preparations. Mackamide CMA will help enhance the viscosity response of the .. |
|||
Melting Point | 60.0 - 64.0 °C | 140 - 147 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 103 Linear Thermoplastic Polyurethane Pearlbond™ 103 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity level. I.. |