Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 30.0 - 50.0 °C | 86.0 - 122 °F | |
BASF Diisopropanolamine S Formula: C6H15NO2CAS: 110-97-4Description: Diisopropanolamine S is a colorless to yellow solid or melt with an amine-like odor. It is fully soluble in water.Synonyms: DIPA, 1,1’-Iminobis[2-propano.. |
|||
Melting Point | 46.0 - 50.0 °C | 115 - 122 °F | |
BASF Hydroxypivalic Acid Neopentylglycolester (HPN Formula: C10H20O4CAS: 1115-20-4Description: Hydroxypivalic Acid Neopentylglycolester (HPN) is a colorless, odorless solid.Synonyms: Neopentyl glycol monohydroxypivalate, Hydroxyneopentyl hydroxypiva.. |
|||
Melting Point | 46.0 - 50.0 °C | 115 - 122 °F | |
BASF Hydroxypivalic Acid Neopentylglycolester Molten (HPN) Formula: C10H20O4CAS: 1115-20-4Description: Hydroxypivalic Acid Neopentylglycolester Molten (HPN) is a colorless, odorless molten solid. Synonyms: Neopentyl glycol monohydroxypivalate, Hydroxyneopen.. |
|||
Melting Point | 30.0 - 50.0 °C | 86.0 - 122 °F | |
BASF Diisopropanolamine Formula: C6H15NO2CAS: 110-97-4Description: Diisopropanolamine is a colorless to yellow solid or melt with an amine-like odor. It is fully soluble in water.Synonyms: DIPA, 1,1’-Iminobis[2-propanol].. |