Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 360 - 382 °C | 680 - 720 °F | |
PolyOne Trilliant™ HC HC9820-0030 RS Natural Polyetheretherketone (PEEK) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |