Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 304 - 370 °C | 579 - 698 °F | |
Johnson Matthey JM A5 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |