Polymer Property : Melting Point = 342 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 321 - 342 °C
610 - 648 °F
Average value: 327 °C Grade Count:16
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum..
Melting Point 327 - 342 °C
621 - 648 °F
Zeus PTFE Tubing
Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,..