Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 200 - 228 °C | 392 - 442 °F | Average value: 224 °C Grade Count:19 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |