Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B GF 15 Polybutylene Terephthalate, 15% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 15% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B GF 20 FRK 3 Polybutylene Terephthalate, 20% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant FeaturesPBT with the content of 20% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 30% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B GF 50 PBT, 50% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 50% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 BT PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 10 FRX 5 PBT reinforced with 10% glass fibre, with flame retardant Features: PBT with the content of 10 % chemically bound glass fibre and with the halogen freeflame retardant. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other ho.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 15 FRX 5 PBT reinforced with 15% glass fibre, with flame retardant Features: PBT with the content of 15 % chemically bound glass fibre and with the halogen freeflame retardant. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other ho.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 20 000/2 PBT, 20% glass fibre FeaturesPBT for injection moulding, pure without lubricant, chemically reinforced with 20% glass fibre, excellent flow. Characterised by excellent properties also at minus temperatures like eg. modu.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 20 PBT, 20% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 45 PBT, 45% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 45% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B2 GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | STN EN 11357-1 |
Plastcom SLOVASTYR® B BT BK PBT Regranulate PBT basic type for injection molding. Melt is characterized by very good fluidity, which enables injection molding of complicated and divided products also on multiple moulds. Anisotropy.. |
|||
Melting Point | 210 - 220 °C | 410 - 428 °F | ISO 11357-1 |
Radici Radilon® CST 38FL (dry) Copolyamide 6 semiaromatic Radilon® CS can be used for blown film extrusion in general as well as being particularly suited for co-extrusion with PE because it improves the transparency and thermoformability of the film.Appl.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B FRN 3 LS PBT, flame retarder, light stable FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B GB 20 M PBT, 20% glass beads FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B GF 30 FRL 4 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 6 PBT, 6% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 HML GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 110 - 220 °C | 230 - 428 °F | Average value: 214 °C Grade Count:19 |
Overview of materials for Nylon 6 Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6 Fiber". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Melting Point | 218 - 220 °C | 424 - 428 °F | crystalline melting point; Hot Stage Microscope |
Honeywell Capran® 512 LL Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 512 LL is a heat-stabilized blown film produced from low lactam nylon-6 resin. It is recommended as bagging film for advanced composite fabrication and other high temperature .. |
|||
Melting Point | 218 - 220 °C | 424 - 428 °F | crystalline melting point; Hot Stage Microscope |
Honeywell Capran® 518 LL Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 518 LL is a green tinted, heat-stabilized blown film produced from low lactam nylon-6 resin. It is recommended as bagging film for advanced composite fabrication and other hig.. |
|||
Melting Point | 217 - 220 °C | 423 - 428 °F | |
Indium Corp. Indalloy® 256 96.5Sn/3.0Ag/0.5Cu Lead-Free Solder Alloy Referred to as the SAC305 alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | ISO R 1218 |
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Conditioned Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | ISO R 1218 |
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Dry Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Melting Point | 208 - 220 °C | 406 - 428 °F | |
Shandong Guangyin PA 610 Nylon Resin Features and Applications: Compared with nylon 6 and nylon 66, nylon 610 is much softer and lower in water absorption, featured by excellent low temperature resistance and dimensional stability. Due.. |
|||
Melting Point | 216 - 220 °C | 420 - 428 °F | |
Chase Plastics CP Pryme® N140MGHL (Dry) Nylon 6, 40% Glass Fiber Reinforced, Heat Stabilized, Lubricated Features: Heat StabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Melting Point | 216 - 220 °C | 420 - 428 °F | Average value: 220 °C Grade Count:24 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |