Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 182 - 193 °C | 360 - 379 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® 16N92 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N92 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can b.. |
|||
Melting Point | 183 - 193 °C | 361 - 379 °F | MQSA 114 |
Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This gra.. |
|||
Melting Point | 171 - 193 °C | 340 - 380 °F | |
Hexcel® HexWeb® TPU™ Thermoplastic Polyurethane Honeycomb Designation: Material-Cell Size (inches)-Film Gauge (inches)-Outer Skin Thickness.HexWeb® TPU™ is an attractive thermoplastic urethane honeycomb that has been developed using a proprietary fusing .. |
|||
Melting Point | 171 - 193 °C | 340 - 380 °F | ASTM D789 |
Adell ER-17 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |