Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 138 - 148 °C
280 - 298 °F
MQSA 111
Lubrizol Advanced Materials PEARLTHANE® 12K85LB Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 12K85 LB is a standard polyester-based TPU with a lubricating additive, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mech..
Melting Point 138 - 148 °C
280 - 298 °F
Fine Organics FINAWAX C Lubricant Additive
Applications: Antiblock agent for soft PVC films/sheets, strong release agent for rigid PVC calendered sheets, dispersant for FRLS PVC compounds.Information provided by Fine Organics
Melting Point 142 - 148 °C
288 - 298 °F
DSC; ISO 3146
Borealis BorPure™ RD226CF Polypropylene Random Copolymer
BorPure™ RD226CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD226CF is recommended for food packaging..
Melting Point 142 - 148 °C
288 - 298 °F
DSC; ISO 3146
Borealis BorPURE™ RD266CF Polypropylene Random Copolymer
BorPure™ RD266CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD266CF is recommended for food packaging..
Melting Point 142 - 148 °C
288 - 298 °F
DSC; ISO 3146
Borealis BorPURE™ RE216CF Polypropylene Random Copolymer
BorPure™ RE216CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: BorPure™ RE216CF is recommended for Lamination films, Me..