Melting Point 1370 - 1418 °C
2500 - 2584 °F
Haynes Hastelloy® B-3® alloy, 0% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Melting Point 1370 - 1418 °C
2500 - 2584 °F
Haynes Hastelloy® B-3® alloy, 10% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Melting Point 1370 - 1418 °C
2500 - 2584 °F
Haynes Hastelloy® B-3® alloy, 20% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Melting Point 1370 - 1418 °C
2500 - 2584 °F
Haynes Hastelloy® B-3® alloy, 30% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Melting Point 1370 - 1418 °C
2500 - 2584 °F
Haynes Hastelloy® B-3® alloy, 40% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Melting Point 1370 - 1418 °C
2500 - 2584 °F
Haynes Hastelloy® B-3® alloy, 50% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Melting Point 1370 - 1418 °C
2500 - 2584 °F
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea..