Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1257 - 1356 °C | 2295 - 2473 °F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 732°C (1350°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Melting Point | 1257 - 1356 °C | 2295 - 2473 °F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 732°C/8hr/FC to 621°C/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Melting Point | 1257 - 1356 °C | 2295 - 2473 °F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Aged 732°C (1350°F)/4hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Melting Point | 1257 - 1356 °C | 2295 - 2473 °F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Aged 732°C (1350°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Melting Point | 1257 - 1356 °C | 2295 - 2473 °F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Cold Drawn 37.5% Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Melting Point | 1257 - 1356 °C | 2295 - 2473 °F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Cold Drawn 37.5% Plus Aging 649°C (1200°F)/4hr/FC to 579°C/4hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Melting Point | 1257 - 1356 °C | 2295 - 2473 °F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 718°C (1325°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Melting Point | 1257 - 1356 °C | 2295 - 2473 °F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 746°C (1375°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Melting Point | 1246 - 1356 °C | 2275 - 2473 °F | |
Kennametal Stellite Stellite® 4 Cobalt Chromium Alloy The higher tungsten content of Stellite alloy 4 gives improved high temperature properties and an increase in abrasive wear resistance over Stellite alloy 6, but not as good as Stellite alloy 12 or .. |