Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1271 - 1343 °C | 2320 - 2449 °F | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725) Age Hardened Strip Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Strip samples. Other property values are typical of INCONEL® alloy 725.D.. |
|||
Melting Point | 1271 - 1343 °C | 2320 - 2449 °F | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Round Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Round samples. Other property values are typical of INCONEL® alloy 725.D.. |
|||
Melting Point | 1271 - 1343 °C | 2320 - 2449 °F | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Tube Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Age Hardened Tube samples. Other property values are typical of INCONEL® alloy 725.Data provi.. |
|||
Melting Point | 1271 - 1343 °C | 2320 - 2449 °F | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Annealed Round Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Round samples. Other property values are typical of INCONEL® alloy 725.Data provided.. |
|||
Melting Point | 1271 - 1343 °C | 2320 - 2449 °F | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Annealed Tube Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Tube samples. Other property values are typical of INCONEL® alloy 725.Data provided .. |
|||
Melting Point | 1260 - 1343 °C | 2300 - 2449 °F | |
Special Metals INCONEL® G-3 Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Melting Point | 1260 - 1343 °C | 2300 - 2449 °F | |
ATI Allvac® 718Plus™ Nickel Superalloy Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the.. |