Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 134 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 130 - 134 °C
266 - 273 °F
ASTM D3418
Arkema Group Kynar Flex® 2950 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Melting Point 130 - 134 °C
266 - 273 °F
ISO 3146
Borealis Borseal™ TD120BF Terpolymer for BOPP Film
Borseal TD120BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD120B..
Melting Point 130 - 134 °C
266 - 273 °F
ISO 3146
Borealis Borseal™ TD220BF Terpolymer for BOPP Film
Borseal TD220BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD220B..
Copyright © lookpolymers.com All Rights Reserved