Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 105 - 126 °C | 221 - 259 °F | Average value: 118 °C Grade Count:8 |
Overview of materials for Polybutene This property data is a summary of similar materials in the MatWeb database for the category "Polybutene". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Melting Point | 124 - 126 °C | 255 - 259 °F | |
Indium Corp. Indalloy 67 Bismuth-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 110 - 126 °C | 230 - 259 °F | |
3M Dyneon™ Dynamar™ FX 5911 Polymer Processing Additive Dynamar FX 5911 is a free-flowing fluoropolymer processing aid that is designed for use at very low levels (typically 250-1000 ppm) necessary to improve processing, it does not alter or detract from.. |
|||
Melting Point | 110 - 126 °C | 230 - 259 °F | |
3M Dyneon™ FX 5912 Dynamar™ Polymer Processing Additive Dynamar FX 5912 is a free-flowing fluorothermoplastic processing aid that is designed for use at very low levels to improve the processing of thermoplastics. Typical use levels of 200 to 1000 ppm ha.. |