Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1138 - 1220 °C | 2080 - 2220 °F | |
Kennametal Stellite Delcrome® 93 Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Highly alloyed white cast iron, abrasion resistant. Carbides in a martensitic matrix offer high.. |
|||
Melting Point | 1075 - 1220 °C | 1967 - 2230 °F | |
Kennametal Stellite Nucalloy® 488V High-Silicon Nickel-Base Hardfacing Alloy Applications include diesel engine valves, and injection mold screws.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinati.. |
|||
Melting Point | 1150 - 1220 °C | 2100 - 2230 °F | |
Wieland 1751 Wilaform Palladium Approach-steady palladium alloy for nearly all purposes in decoration manufacturingApplications: casting, chains, laminar decoration, pipes, tubingDental |