Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1038 - 1082 °C | 1900 - 1980 °F | |
Materion Brush 1915â„¢ Annealed Temper Rod Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Melting Point | 1038 - 1082 °C | 1900 - 1980 °F | |
Materion Brush 1915â„¢ Hard Temper Rod, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Melting Point | 1038 - 1082 °C | 1900 - 1980 °F | |
Materion Brush 1915™ AT Temper Rod Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Melting Point | 1038 - 1082 °C | 1900 - 1980 °F | |
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Melting Point | 1038 - 1082 °C | 1900 - 1980 °F | |
Materion Brush 1915™ Heat Treated Temper Rod, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Melting Point | 1038 - 1082 °C | 1900 - 1980 °F | |
Materion Brush 1915™ Heat Treated Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Melting Point | 644 - 1082 °C | 1190 - 1980 °F | |
Materion AlBeMet® AM 162 Rolled Sheet, Annealed Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are.. |