Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 980 - 1040 °C
1800 - 1900 °F
Osprey Metals HTN 3 Brazing Powder
Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme..
Melting Point 980 - 1070 °C
1800 - 1960 °F
Osprey Metals HTN 4 Brazing Powder
Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme..
Melting Point 980 - 1010 °C
1800 - 1850 °F
Osprey Metals HTN 8 Brazing Powder
Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme..
Melting Point 980 - 1240 °C
1800 - 2260 °F
Kennametal Stellite Nucalloy® 453 High-Silicon Nickel-Base Hardfacing Alloy
Applications include chemical control valves, nuclear globe valves, nuclear gate valves, nuclear sliding parts, and pressure bars for plywood cutters.Nucalloy® alloys are unique, patented, high-s..
Melting Point 980 - 1040 °C
1800 - 1900 °F
Wieland 1909 Wilaform Gold
Hard palladium white gold alloy with beautiful white color.Applications: casting, chains, laminar decoration, pipes, tubingDental
Melting Point 980 °C
1800 °F
Goodfellow Copper 56.4/Titanium 43.6 Alloy
Information provided by Goodfellow.
Melting Point 980 °C
1800 °F
Goodfellow Copper 87/Zirconium 13 Alloy
Information provided by Goodfellow.
Melting Point <= 980 °C
<= 1800 °F
CMW® D154X Post-Oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3
For electrical contacts; resistant to welding and high surge currents.Information provided by CMW Inc.
Melting Point <= 980 °C
<= 1800 °F
CMW® D158F Silver Graphite Contact Material
For electrical contacts; reduced sticking, low frictionInformation provided by CMW Inc.
Melting Point <= 980 °C
<= 1800 °F
CMW® D54 Silver Cadmium Oxide Contact Material ASTM B781, Table 2, Type B
For electrical contacts; especially resistant to welding and high surge currentsInformation provided by CMW Inc.
Melting Point <= 980 °C
<= 1800 °F
CMW® D54F Pre-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3
For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc.
Melting Point <= 980 °C
<= 1800 °F
CMW® D55F Pre-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3
For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc.
Melting Point <= 980 °C
<= 1800 °F
CMW® D55X Post-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3
For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc.
Melting Point <= 980 °C
<= 1800 °F
CMW® D581F Silver Graphite Contact Material
For electrical contacts; reduced sticking, low friction.Information provided by CMW Inc.
Melting Point >= 980 °C
>= 1800 °F
CMW® ELKONITE® 1060 Silver Tungsten Carbide Contact Material
Electrical contactor material for medium current ac applicationsInformation provided by CMW Inc.
Melting Point 980 - 3410 °C
1800 - 6170 °F
CMW® ELKONITE® 20S Infiltrated Tungsten Silver Contact Material ASTM B531, Class A, infiltrated
For electrical contacts resistant to arcing and welding in circuit breakers, etc.Information provided by CMW Inc.
Melting Point >= 980 °C
>= 1800 °F
CMW® ELKONITE® 3042 Silver Tungsten Carbide contact material ASTM B663
For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc.
Melting Point >= 980 °C
>= 1800 °F
CMW® ELKONITE® 30S Silver Tungsten contact material ASTM B631
For electrical contacts, circuit breakers. Resistant to arcing and welding.Information provided by CMW Inc.
Melting Point >= 980 °C
>= 1800 °F
CMW® ELKONITE® 3150 Silver Tungsten Carbide contact material ASTM B663 Table 2, Class B
For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc.
Melting Point 980 - 3410 °C
1800 - 6170 °F
CMW® ELKONITE® 35S Silver Tungsten contact material ASTM B631, Class B, infiltrated
For arcing and current carrying electrical contacts; household and power circuit breakers.Information provided by CMW Inc.
Melting Point 980 - 3410 °C
1800 - 6170 °F
CMW® ELKONITE® 40S Infiltrated Tungsten Silver contact material ASTM B631
For arcing and current carrying electrical contacts.Information provided by CMW Inc.
Melting Point 980 - 3410 °C
1800 - 6170 °F
CMW® ELKONITE® 45S Infiltrated Tungsten Silver contact material ASTM B631
For arcing and current carrying electrical contacts.Information provided by CMW Inc.
Melting Point 980 - 3410 °C
1800 - 6170 °F
CMW® ELKONITE® 50S Infiltrated Tungsten Silver contact material ASTM B631, Class C, infiltrated
For arcing and current carrying electrical contacts.Information provided by CMW Inc.
Melting Point <= 980 °C
<= 1800 °F
CMW® D582F Silver Graphite Contact Material
For electrical contacts; reduced sticking, low voltage DCInformation provided by CMW Inc.
Melting Point 980 - 2610 °C
1800 - 4730 °F
CMW® ELKONITE® 7065 Infiltrated Molybdenum Silver contact material ASTM B662 Table 1, Class A1
For arcing electrical contactsInformation provided by CMW Inc.
Melting Point 980 - 2610 °C
1800 - 4730 °F
CMW® ELKONITE® 7165 Molybdenum Silver contact material
For arcing electrical contactsInformation provided by CMW Inc.
Melting Point >= 980 °C
>= 1800 °F
CMW® ELKONITE® G13 Tungsten Carbide Silver contact material ASTM 663, Class B, infiltrated
For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc.
Melting Point >= 980 °C
>= 1800 °F
CMW® ELKONITE® G14 Tungsten Carbide Silver contact material ASTM 663, Class A, infiltrated
For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc.
Melting Point >= 980 °C
>= 1800 °F
CMW® ELKONITE® TC20 Tungsten Carbide Copper material
For electroforging and electrical upsetting dies.Information provided by CMW Inc.
Melting Point >= 980 °C
>= 1800 °F
CMW® ELKONITE® TC5 Tungsten Carbide Copper material
For wiping and arcing electrical contacts and light duty welding tips.Information provided by CMW Inc.