Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 84.0 °C | 183 °F | Internal Method |
Polimeri Europa Greenflex® FF 55 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 55 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 55 show high flexibility.Main Applications: Greenflex FF 55 is recommended f.. |
|||
Melting Point | 84.0 °C | 183 °F | DSC |
Westlake EMAC® SP2242 Specialty Copolymer
(discontinued **) EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo.. |
|||
Melting Point | 84.0 °C | 183 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 30707HS Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
(discontinued **) 7 wt% Acrylic Acid.Nucrel® 30707HS is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio.. |
|||
Melting Point | 84.0 °C | 183 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3121A Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 7.5 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dr.. |
|||
Melting Point | 84.0 °C | 183 °F | Exxon Method |
ExxonMobil Iotek® 7020 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas.. |
|||
Melting Point | 84.0 °C | 183 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 0903HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0903HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Melting Point | 84.0 °C | 183 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 0908HS Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating 9.2 wt% Methacrylic Acid.Nucrel® 0908HS is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and blown/cast film operations desi.. |
|||
Melting Point | 84.0 °C | 183 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 0910HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating 8.7 wt% Methacrylic Acid.Nucrel® 0910HS (High-Stability) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating and extrusion lamin.. |
|||
Melting Point | 84.0 °C | 183 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 407 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating 4 wt% Methacrylic Acid.Nucrel® 0407 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment desi.. |
|||
Melting Point | 84.0 °C | 183 °F | ASTM D3418, ISO 3146 |
DuPont™ Elvax® 440 Ethylene Vinyl Acetate DuPont™ Elvax® 440 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. ELVAX® 440 EVA Resin complies with Food and Drug Administration Regulation 21 CFR 177.1350(a)(1.. |
|||
Melting Point | 84.0 °C | 183 °F | DSC |
DuPont™ Surlyn® 8150 Ionomer Resin, Sodium Surlyn® 8150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA content and .. |
|||
Melting Point | 84.0 °C | 183 °F | DSC |
Arkema Group LOTADER® 3430 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 3430 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 3430 is a versatile adhesive for extrusion coating or lam.. |
|||
Melting Point | 84.0 °C | 183 °F | 10°C/min |
Arkema Group Evatane® 1350 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for molding very flexible articles. Examples: gaskets.ISO data provided by the manufacturer, Arkema. |
|||
Melting Point | 84.0 °C | 183 °F | ASTM D3417 |
DuPont Elvax® 3176CW-3 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 3176CW-3 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additi.. |
|||
Melting Point | 84.0 °C | 183 °F | Exxon Method |
ExxonMobil Iotek® 8020 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature .. |
|||
Melting Point | 84.0 °C | 183 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 0910HS-SR Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating
(discontinued **)< 8.7 wt% Methacrylic Acid.Nucrel® 0910HS-SR is an ethylene-methacrylic acid copolymer resin available for use in conventional and coextrusion coating equipment designed to process polyethylene resin.. |
|||
Melting Point | 84.0 °C | 183 °F | Exxon Method |
ExxonMobil Escorene® LD-724 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty compounding applications. Outstanding heat sealability along with excellent strength properties .. |