Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 82.0 - 94.0 °C | 180 - 201 °F | ASTM D3418(DSC) |
DuPont Nucrel® 535 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 535 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Melting Point | 82.0 °C | 180 °F | by DSC; ASTM D3418 |
Westlake EMAC® SP2405 20% Ethylene-Methyl Acrylate Copolymer
(discontinued **) Westlake EMAC® SP2405 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperature are required. SP2405 provides.. |
|||
Melting Point | 82.0 °C | 180 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3129 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 10 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Melting Point | 82.0 °C | 180 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3120 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 7.5 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dr.. |
|||
Melting Point | 82.0 °C | 180 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 910 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating 8.7 wt% Methacrylic Acid.Nucrel® 0910 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment de.. |
|||
Melting Point | 82.0 °C | 180 °F | TRN-14 |
Tipco Tipcolite® TPF 1911 - Cashew Nut (CNSL) Modified Phenolic Resin with 51 mm Norton Flow, with 7% Hexamine Cashew Nut (CNSL) Modified Phenolic Resin with 51mm Norton FlowApplications: Nitrile RubberProcessing: CompoundingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Melting Point | 82.0 °C | 180 °F | by DSC; ASTM D3418 |
Westlake EMAC® SP2205 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2205 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2205 provide.. |
|||
Melting Point | 82.0 °C | 180 °F | by DSC; ASTM D3418 |
Westlake EMAC® SP2220 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2220 is a 20% EMA copolymer designed for compounding, extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficien.. |
|||
Melting Point | 82.0 °C | 180 °F | ASTM D3418 |
Westlake EMAC® SP2255 17% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2255 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s.. |
|||
Melting Point | 82.0 °C | 180 °F | ASTM D3418 |
Westlake EMAC® SP2258 17% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2258 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s.. |
|||
Melting Point | 82.0 °C | 180 °F | DSC; ASTM-D3418 |
Westlake EMAC® SP2409 20% EMA Copolymer Westlake EMAC� SP2409 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or a high coefficient of fr.. |
|||
Melting Point | 82.0 °C | 180 °F | DTA |
DuPont™ Surlyn® 8020 Ionomer Resin, Sodium Surlyn® 8020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Melting Point | 82.0 °C | 180 °F | DSC |
DuPont™ Surlyn® 9150 Ionomer Resin, Zinc Surlyn® 9150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The high MAA content and mi.. |
|||
Melting Point | 82.0 °C | 180 °F | DSC |
Arkema Group EVATANE® 20-20 Copolymer Ethylene - Vinyl Acetate EVATANE® 20-20 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 20-20 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Melting Point | 82.0 °C | 180 °F | by DSC |
Westlake EMAC® SP 1257 Ethylene-Methyl Acrylate Copolymer
(discontinued **) 20% Methyl Acrylate Content. Characteristics: FDA Clearance for Packaging of Most Foods, Including Aseptic Packaging; Less Crystalline and Softer than Polyethylene; Excellent Heat Stability Allows .. |
|||
Melting Point | 82.0 °C | 180 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 2169 Anhydride-Modified Ethylene Acrylate Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |