Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 79.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 79.0 °C
174 °F
Freezing Point via DSC/ASTM D3418
DuPont Nucrel® 1302 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film  (discontinued **)
13 wt% Methacrylic Acid.Nucrel® 1302 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process po..
Melting Point 79.0 °C
174 °F
Freezing Point via DSC/ASTM D3418
DuPont Appeel® LSR 11D569 Modified EVA Lidding Sealing Resin  (discontinued **)
Appeel 11D569 is a modified ethylene vinyl acetate copolymer resin designed to be used as a sealing layer for lidding applications. It provides peelable seals to a variety of surfaces including poly..
Melting Point 79.0 - 89.0 °C
174 - 192 °F
Fine Organics FINALUX G1 Lubricant Additive
Applications:Lubricant for:rigid PVC pipesconduitsfittingscable compoundsInformation provided by Fine Organics
Melting Point 79.0 °C
174 °F
Eutectic
Indium Corp. Indalloy® 174 Bi-In-Sn Fusible Alloy
Environmentally safe fusible alloy. Contains no lead or cadmium.Information provided by the manufacturer, Indium Corporation.
Melting Point 79.0 - 85.0 °C
174 - 185 °F
Struktol TR 131 Slip Agent, Lubricant, Mold Release Agent
Unsaturated primary amide derived from erucic acid.STRUKTOL® TR 131 is mainly used as a slip agent in polyolefin films, reducing the coefficient of friction. It is the agent of choice at higher e..
Melting Point 79.0 °C
174 °F
Peak; Westlake Method
Westlake Elevate™ EF526 16% Ethylene Vinyl Acetate Copolymer
Westlake Elevate™ EF526 resin is a 16% EVA copolymer designed for cast film, extrusion coatings, and thermal laminations.Application/UsesThermal laminationsCast FilmExtrusion CoatingsThis resin gra..
Melting Point 79.0 °C
174 °F
ASTM D3418
Westlake EMAC® SP2252 20.5% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2252 is a 20.5% EMA copolymer containing slip and antiblock. This resin is designed for blown film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal te..
Melting Point 79.0 °C
174 °F
Freezing Point via DSC/ASTM D3418
DuPont Elvax® 3124 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating
9 wt% Vinyl Acetate.Elvax® 3124 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins...
Melting Point 79.0 - 81.0 °C
174 - 178 °F
BASF Triphenylphosphine Pellets
Formula: C18H15PCAS: 603-35-0Description: Triphenyl phosphine pellets are a colorless solid, and have a faint specific odor. It is insoluble with water. Synonyms: TPP, Triphenylphosphane, Triphenyl..
Melting Point 79.0 - 81.0 °C
174 - 178 °F
BASF Triphenylphosphine Molten
Formula: C18H15PCAS: 603-35-0Description: Triphenyl phosphine pellets are a colorless solid, and have a faint specific odor. It is insoluble with water.Synonyms: TPP, Triphenylphosphane, Triphenylp..
Melting Point 79.0 °C
174 °F
Upon Melting via DSC/ASTM D3418
DuPont Appeel® LSR 2044 Modified EVA Lidding Sealing Resin
Appeel® 2044 is a blown or cast film resin designed to be a sealing layer for lidding applications. It provides a peelable seal over a broad temperature range to a number of container materials inc..