Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 77.0 °C | 171 °F | ISO 11357-3 |
Total Evatane® 24 - 03 HDPE vinyl acetate copolymer, blown film, injection molding
(discontinued **) EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 130 to 160.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f.. |
|||
Melting Point | 77.0 °C | 171 °F | Exxon Method |
ExxonMobil Escorene® LD-737 EVA Copolymer for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 19.5% vinyl acetate copolymer.Applications: Compound viscosity modifier; High flow applications. |
|||
Melting Point | 77.0 °C | 171 °F | Exxon Method |
ExxonMobil Escorene® LD-740 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty film and compounding applications. Outstanding heat sealability along with excellent strength pr.. |
|||
Melting Point | 77.0 - 82.0 °C | 171 - 180 °F | |
Indium Corp. Indalloy 28 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 77.0 °C | 171 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3135SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 12 wt% Vinyl Acetate.Elvax® 3135SB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Melting Point | 77.0 °C | 171 °F | Freezing Point; DSC; ASTM-D3418 |
Westlake EF532 12% EVA Copolymer (Experimental Product) Westlake EF532 resin is a 12.0% EVA copolymer designed for use as a sealant / lamination layer in monolayer or coextruded flexible film structures. It has very low seal initiation temperature, excel.. |
|||
Melting Point | 77.0 °C | 171 °F | Freezing Point |
Westlake Elevate™ DA532 Ethylene Vinyl Acetate Copolymer Experimental ProductDescription: Westlake DA532 resin is a 12.0% EVA copolymer designed for use as a sealant / lamination layer in monolayer or coextruded flexible film structures. It has very low .. |
|||
Melting Point | 77.0 °C | 171 °F | by DSC; ASTM D3418 |
Westlake EMAC® SP2260 24% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2260 is a 24% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2260 provide.. |
|||
Melting Point | 77.0 °C | 171 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3190 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 25 wt% Vinyl Acetate.Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melting Point | 77.0 °C | 171 °F | Freezing Point; ASTM D3418 |
DuPont™ Bynel® 30E783 Anhydride Modified Ethylene Vinyl Acetate BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 77.0 °C | 171 °F | D.S.C. method |
Arkema Group Orevac® 9304 Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group |
|||
Melting Point | 77.0 °C | 171 °F | ASTM-D3418 |
Braskem Evateno® HM 728 EVA Hot Melt Copolymer Evateno® HM 728 is a copolymer of Ethylene-Vinyl Acetate (EVA) with high vinyl-acetate content, medium molecular weight, and good compatibility with other thermoplastic and elastomeric resins. Evat.. |
|||
Melting Point | 77.0 °C | 171 °F | DSC |
Arkema Group LOTADER® 4403 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4403 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. LOTADER 4403 is a versatile adhesive for extrusion lamination, de.. |
|||
Melting Point | 77.0 - 78.0 °C | 171 - 172 °F | |
BASF 2-Ethyl Imidazole Formula: C5H8N2CAS: 1072-62-4Description: 2-Ethyl Imidazole is a colorless to yellowish solid with an amine-like odor.Synonyms: 2EIApplications: It is used as a Pharmaceuticals, Crop protection agen.. |
|||
Melting Point | 77.0 °C | 171 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 20E482 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Melting Point | 77.0 °C | 171 °F | Freezing Point; ASTM D3417 |
DuPont Elvax® 3135B Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 3135B is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additive:.. |
|||
Melting Point | 77.0 °C | 171 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3190LG Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
(discontinued **) 25 wt% Vinyl Acetate.Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |