Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 70.0 °C | 158 °F | Exxon Method |
ExxonMobil Escorene® LD-767 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low gel 29.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile.. |
|||
Melting Point | 70.0 °C | 158 °F | Exxon Method |
ExxonMobil Escorene® LD-770 Very High Flow EVA Resin for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A relatively low viscosity ethylene vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance, at the same viscosity of.. |
|||
Melting Point | 70.0 °C | 158 °F | DSC |
DuPont™ Surlyn® 9320W Ionomer Resin, Zinc
(discontinued **) Surlyn® 9320W thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. This very low modulus zinc.. |
|||
Melting Point | 70.0 - 80.0 °C | 158 - 176 °F | |
Fine Organics FINALUX G 211 Lubricant Additive Applications: External lubricants for rigid and soft PVC, specially for Ba-Cd stabilized PVC products.Information provided by Fine Organics |
|||
Melting Point | 70.0 - 80.0 °C | 158 - 176 °F | |
Fine Organics FINALUX G 411 Lubricant Additive Applications: Compatible lubricant for rigid PVC preferable for use in glass clear rigid PVC articles, lubricant for duroplast.Information provided by Fine Organics |
|||
Melting Point | 70.0 - 102 °C | 158 - 216 °F | |
Indium Corp. Indalloy 43 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 70.0 - 105 °C | 158 - 221 °F | |
Indium Corp. Indalloy 47 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 70.0 - 123 °C | 158 - 253 °F | |
Indium Corp. Indalloy 65 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 70.0 - 80.0 °C | 158 - 176 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 104 Linear Thermoplastic Polyurethane Pearlbond™ 104.is a linear, aromatic polyurethane, supplied in form of small white or slightly yellowish granules, which combines a high crystallisation rate with a high thermoplasticity level... |
|||
Melting Point | 70.0 - 73.0 °C | 158 - 163 °F | |
Indium Corp. Indalloy 24 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 70.0 - 78.0 °C | 158 - 172 °F | |
Indium Corp. Indalloy 26 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 70.0 °C | 158 °F | Eutectic |
Indium Corp. Indalloy® 158 Bi-Pb-Sn-Cd Solder Alloy Lowest melting point solder. Good fusible alloy used for lens blocking.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 70.0 °C | 158 °F | |
Synergy Polymers Ultra Purge HIGH-E Best with color changes and material changes. Cleans out barrels, nozzles, hot runners, and heads of extruders from carbon remnants, deposits and incrustations. Has expanding agents to help in clean.. |
|||
Melting Point | 70.0 °C | 158 °F | |
Synergy Polymers Ultra Purge Plus Best with color changes and material changes. Cleans out barrels, nozzles, hot runners, and heads of extruders from carbon remnants, deposits and incrustations. Has expanding agents. Moldable compou.. |
|||
Melting Point | 70.0 °C | 158 °F | |
Synergy Polymers Ultra Purge P-O Ultra Purge is a specially designed cleaning compound that comes premixed and ready-to-use in pellet form. It cleans black specks and deposits from screws, barrels, nozzle, hot runners and heads of .. |
|||
Melting Point | 70.0 - 76.0 °C | 158 - 169 °F | |
Struktol TR 121 Slip Agent, Lubricant, Mold Release Agent Unsaturated fatty primary amide derived from oleic acid.One of the major uses of oleamide is as a slip agent in polyethylene films. It functions by migrating to the film surface in a microscopic coa.. |
|||
Melting Point | 70.0 - 75.0 °C | 158 - 167 °F | |
Solvay ALKAMULS® 504/V Surfactant Chemical Name: ETHYLENE GLYCOL DISTEARATECAS: 627-83-8Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Ethylene glycol distearate is widely used in cosmetics as pearl.. |
|||
Melting Point | 70.0 °C | 158 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3180 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 28 wt% Vinyl Acetate.Elvax® 3180 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melting Point | 70.0 °C | 158 °F | TRN-14 |
Tipco Tipcolite® TPF 1011 - Unreinforced Thermoset Phenolic Resin, 43 mm Norton Flow without Hexamine Unreinforced Phenolic Resin having 43mm Norton Flow, in Lump FormApplications: General PurposeProcessing: General PurposeInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Melting Point | 70.0 °C | 158 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Bynel® 1124 Modified EVA Adhesive Resin Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Melting Point | 70.0 °C | 158 °F | Exxon Method |
ExxonMobil EXACT™ 4053 Cast Plastomer Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly.. |
|||
Melting Point | 70.0 °C | 158 °F | Peak Melting, Exxon Method |
ExxonMobil EXACT™ 4053 Plastomer for Film Applications Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly.. |
|||
Melting Point | 70.0 °C | 158 °F | ASTM D3418, ISO 3146 |
DuPont™ Surlyn® 9320 Zinc Ionomer Surlyn® 9320 is a zinc ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 9320 thermoplastic resin .. |
|||
Melting Point | 70.0 °C | 158 °F | Dow Method |
Dow AFFINITY™ GA 1950 Polyolefin Plastomer (POP) AFFINITY™ GA 1950 Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. This product can be used in applications such as polymer modification (i.e. flow enhancement and.. |
|||
Melting Point | 70.0 °C | 158 °F | ASTM D3418, ISO 3146 |
DuPont™ Surlyn® 6320 Magnesium Ionomer Surlyn® 6320 is a magnesium ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 6320 thermoplastic r.. |
|||
Melting Point | 70.0 °C | 158 °F | |
Arkema Group OREVAC® 18630 Maleic Anhydride Modified Ethylene - Acrylate Copolymer OREVAC® 18630 is anhydride modified Ethylene – Acrylate copolymer. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) .. |
|||
Melting Point | 70.0 - 103 °C | 158 - 217 °F | Average value: 89.8 °C Grade Count:9 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a.. |
|||
Melting Point | 70.0 °C | 158 °F | ASTM D3417- ISO 3146 |
DuPont Elvax® CM4875 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® CM4875 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Specialty grades of Elvax® have the unusual combination of high vinyl acetate levels and low.. |