Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 682 - 699 °C | 1260 - 1290 °F | |
Lucas-Milhaupt BRAZE 495 Carbide Brazing Alloy Applications: Because of its excellent wetting properties, Braze 495 is used extensively for brazing tungsten carbide inserts to cutting tools and rock drills. It may be used for joining all types .. |
|||
Melting Point | 682 - 743 °C | 1260 - 1370 °F | |
Lucas-Milhaupt Silvaloy® A35 Brazing Alloy Silvaloy A35 is a good general purpose alloy often used when cadmium must be avoided such as in the dairy and food industries. It is used for brazing in the electrical industry and for brazing brass.. |