Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 644 - 1180 °C | 1190 - 2160 °F | |
Materion AlBeMet® AM 162 Extruded Bar, Annealed Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube.. |
|||
Melting Point | 644 - 1082 °C | 1190 - 1980 °F | |
Materion AlBeMet® AM 162 Rolled Sheet, Annealed Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are.. |