Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 607.2 - 618.3 °C | 1125 - 1145 °F | |
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo 45 is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wet.. |
|||
Melting Point | 607.2 - 618.3 °C | 1125 - 1145 °F | |
Lucas-Milhaupt Silvally® 45 Flux Coated Rod Brazing Alloy Silvaloy 45 FC is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joinin.. |
|||
Melting Point | 607.2 - 710 °C | 1125 - 1310 °F | |
Lucas-Milhaupt Silvaloy® 30 Brazing Alloy Silvaloy 30 is historically a modification of Silvaloy 35 with further reduction in silver content resulting in a higher melting point and a longer range. Silvaloy 30 is used for brazing steel, stai.. |
|||
Melting Point | 607.2 - 701.7 °C | 1125 - 1295 °F | |
Lucas-Milhaupt Silvaloy® 35 Brazing Alloy Silvaloy 35 is an alloy with a melting range suitable for brazing steel, stainless steel, copper, copper alloys, nickel, nickel alloys or combinations of these metals. It is free-flowing and suited .. |
|||
Melting Point | 607.2 - 618.3 °C | 1125 - 1145 °F | |
Lucas-Milhaupt Silvaloy® 45 Brazing Alloy Silvaloy 45 is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining s.. |
|||
Melting Point | 607.2 - 710 °C | 1125 - 1310 °F | |
Lucas-Milhaupt EASY FLO 30 Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo 30 is a are good general purpose, low temperature silver brazing filler metals for joining both ferrous and nonferrous metals. Because of their fairly low cost, good fatigue .. |
|||
Melting Point | 607.2 - 746.1 °C | 1125 - 1375 °F | |
Lucas-Milhaupt Silvaloy® 25 Brazing Alloy Silvaloy 25 is historically a modification of Silvaloy 30 with a further reduction in silver content resulting in a higher melting point and a longer melting range. Silvaloy 25 is used for brazing s.. |
|||
Melting Point | 607.2 - 618.3 °C | 1125 - 1145 °F | |
Universal Wire Works BAg-1 (AMS 4769) Silver Brazing Filler Metal Information provided by Universal Wire Works for their line of welding wire and filler metal. |
|||
Melting Point | 607.2 - 701.7 °C | 1125 - 1295 °F | |
Universal Wire Works BAg-2 (AMS 4768) Silver Brazing Filler Metal Information provided by Universal Wire Works for their line of welding wire and filler metal. |
|||
Melting Point | 607.2 - 701.7 °C | 1125 - 1295 °F | |
Lucas-Milhaupt EASY FLO 35 Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo 35 is a are good general purpose, low temperature silver brazing filler metals for joining both ferrous and nonferrous metals. Because of their fairly low cost, good fatigue .. |