Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 567 - 903 °C | 1050 - 1660 °F | |
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |