Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 45.0 - 55.0 °C | 113 - 131 °F | |
Fine Organics FINALUX G 722 Lubricant Additive Applications: Compatible external lubricant for rigid PVC fittings, bottles, films and sheets.Information provided by Fine Organics |
|||
Melting Point | 45.0 - 55.0 °C | 113 - 131 °F | |
Struktol V-PEDS Processing Additive Fatty acid esterTypical Applications: STRUKTOL® V-PEDS has both internal and external lubricant characteristics. It can be used in calendaring, extrusion and injection molding applications. It al.. |
|||
Melting Point | 45.0 °C | 113 °F | ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 742 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Melting Point | 45.0 °C | 113 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3180 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 28 wt% Vinyl Acetate.Elvax® 3180 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melting Point | 45.0 °C | 113 °F | Freezing Point; ASTM D3417 |
DuPont Elvax® 3180Z Ethylene Vinyl Acetate DuPont™ Elvax® 3180Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Applicati.. |