Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 35.0 °C | 95.0 °F | |
Solvay ALKAMULS® 14/R Surfactant Description: Biodegradable nonionic emulsifier, solubiliser for a wide range of formulations. It imparts low temperature stability to EC.Identification: ETHOXYLATED CASTOR OIL CAS: 61791 – 12 â.. |
|||
Melting Point | 35.0 °C | 95.0 °F | |
Solvay ANTAROX® 724/P Surfactant Description: Nonionic EO.PO block polymer. Nonionic emulsifier for liquid formulations. Improves stability and self-emulsifiability. HLB is of 12.8 Identification: ETHOPROPOXYLATED ALKYLPHENOLCAS: 6.. |
|||
Melting Point | 35.0 °C | 95.0 °F | |
Solvay GERONOL® RE/70 Surfactant Description: Multipurpose emulsifier for EC formulations.Identification: BLEND OF FATTY ACIDSSolubility: Insoluble in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, E.. |
|||
Melting Point | 35.0 °C | 95.0 °F | |
Solvay SOPROPHOR® S/25 Surfactant Description: Soprophor® S/25 is Tristyrylphenol ethoxylate, HLB = 14.5. It is nonionic multipurpose high performance emulsifier, soluble in water and most polar and aromatic solvents. Recommended.. |
|||
Melting Point | 35.0 °C | 95.0 °F | |
Solvay SOPROPHOR® TSP/461 Surfactant Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOPROPOXYLATED POLYARYLPHENOLCAS: 70880 – 56 – 7Solubility: Soluble in water and most polar and aromatic sol.. |
|||
Melting Point | <= 35.0 °C | <= 95.0 °F | |
BASF NEOL® Neopentylglycol 90% Solution Formula: C5H12O2CAS: 126-30-7Description: Neol 90% solution is colorless and partially crystalline, with a sweet odor. It is very soluble in water.Applications: Intermediate used in the production .. |