Thermal Properties Metric English Comments
Melting Point 335 °C
635 °F
DSC
Adamas Adalon® 463 PTFE, 15% Special Polyimide
Information provided by Adamas, HPM
Melting Point 335 °C
635 °F
ASTM D789
E-Polymers SEPAZ® C130HS 30% Glass Fiber Reinforced High Temperature Stabilized LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..
Melting Point 335 °C
635 °F
ASTM D789
E-Polymers SEPAZ® C140GP 40% Glass Fiber Reinforced LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..