Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 310 °C | 590 °F | 10°C/min, First Heat; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)
(Unverified Data**) Zytel®® HTNFG52G35HSL BK011 is a 35% glass reinforced, lubricated, heat stabilized high performance polyamide resin, developed for consideration into applications for the food industry. It is also.. |
|||
Melting Point | 310 °C | 590 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Melting Point | 310 °C | 590 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Amodel® AFA-6145 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6145 V0 Z is a 45% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Melting Point | 310 °C | 590 °F | ASTM D4591 |
3M Dyneon™ PFA X 6505 UHP Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA X 6502 UPH, PFA X 6505 UHP and PFA X 6515 UHP are ultra-high purity fluorothermoplastics. These resins were developed for high-purity applications requiring ultra-low levels of metal and .. |
|||
Melting Point | 310 °C | 590 °F | ASTM D4591 |
3M Dyneon™ PFA 6525N Perfluoroalkoxy Fluorothermoplastic
(discontinued **) The excellent chemical temperature resistance of Dyneon™ 6500N PFA is available across a range of melt flow indices, for optimal processability. Dyneon™ PFA 6502N, the highest molecular weight gra.. |
|||
Melting Point | 310 °C | 590 °F | |
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Melting Point | 310 °C | 590 °F | |
Mitsui Arlen™ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Melting Point | 310 °C | 590 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Melting Point | 310 °C | 590 °F | Dry; ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Conditioned) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Melting Point | 310 °C | 590 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Melting Point | 310 °C | 590 °F | ASTM D3418 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Melting Point | 310 °C | 590 °F | Peak; Dry; ASTM D3418 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Conditioned) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Melting Point | 310 °C | 590 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Dry) Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed f.. |
|||
Melting Point | 310 °C | 590 °F | ASTM D3418 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Dry) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Melting Point | 310 °C | 590 °F | DSC |
Solvay Specialty Polymers Hyflon® MFA® XPH 5510_1N Perfluoropolymer Hyflon® XPH 5510_1N is a white aqueous MFA dispersion. Hyflon® XPH 5510_1N exhibits excellent wetting properties and high shear stability. Hyflon® XPH 5510_1N has very good film forming beh.. |
|||
Melting Point | 310 °C | 590 °F | |
Techmer ES Plastiblend® TPX-HTN-000CB 15% Glass Filled Availability: North AmericaForms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Melting Point | 310 °C | 590 °F | Peak; Dry; ASTM D3418 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Melting Point | 310 °C | 590 °F | Dry; ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Melting Point | 310 °C | 590 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HT2VZ-15H PA6T/66-GF15 Information provided by EMS Grivory |
|||
Melting Point | 310 °C | 590 °F | DAM; first heat; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTNFG52G35HSL BK011 is a 35% glass reinforced lubricated heat stabilized high performance polyamide resin developed for consideration into a.. |
|||
Melting Point | 310 °C | 590 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HT2C-3X black 9833 PA6T/66-CF30 Product description: Grivory HT2C-3X black 9833 us a 30% carbon-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc to ISO: PA 6T/66... |
|||
Melting Point | 310 °C | 590 °F | |
3M Dyneon™ PFA 6502 UHPZ Perfluoroalkoxy Fluorothermoplastic Granules Dyneon PFA X 6502 UPH, PFA X 6505 UHP and PFA X 6515 UHP are a new series of ultra-high purity fluorothermoplastics. These resins were developed for high-purity applications requiring ultra-low leve.. |
|||
Melting Point | 310 °C | 590 °F | ASTM D4591 |
3M Dyneon™ PFA 6900GZ Perfluoroalkoxy Fluorothermoplastic Dispersion Dyneon PFA 6900GZ is a 50% solids fluorothermoplastic aqueous dispersion. It is a melt-processable copolymer of tetrafluoroethylene and perfluorinated comonomers, with a melt viscosity several order.. |
|||
Melting Point | 310 °C | 590 °F | |
3M Dyneon™ PFA 6515NZ Perfluoroalkoxy Fluorothermoplastic PFA designed for higher speed or higher shear processing such as injection molding and wire insulation. Demonstrates universal chemical and solvent resistance, high dielectric strength, excellent we.. |
|||
Melting Point | 310 °C | 590 °F | 10°C/min, First Heat; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont .. |
|||
Melting Point | 310 °C | 590 °F | |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Melting Point | 310 °C | 590 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |
|||
Melting Point | 310 °C | 590 °F | ASTM D570 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |
|||
Melting Point | 310 °C | 590 °F | |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), .. |
|||
Melting Point | 310 - 325 °C | 590 - 617 °F | Average value: 313 °C Grade Count:10 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |