Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 282 - 293 °C | 540 - 559 °F | |
PolyOne Trilliant™ HC HC6620-0033 RS Natural Polyamide 66 (Nylon 66) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Melting Point | 282 °C | 540 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Melting Point | 282 °C | 540 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Techtron® PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded (ASTM Product Data Sheet) |
|||
Melting Point | 282 °C | 540 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Techtron® PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Melting Point | 282 °C | 540 °F | ASTM D3417 |
Quantum PPS Information provided by Quantum Advanced Engineering Plastics |
|||
Melting Point | 282 °C | 540 °F | |
Toyobo TS101 PPS, Glass Fiber/Mineral Reinforced Key Feature: High dimensional stabilityHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent.. |
|||
Melting Point | 282 °C | 540 °F | |
Toyobo TS301 PPS, 30% Glass Fiber Reinforced Key Feature: Excellent impact resistance, high flowHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo.. |
|||
Melting Point | 282 °C | 540 °F | |
Toyobo TS401 HS PPS, 40% Glass Fiber Reinforced Key Feature: High toughness, high flow. Features high weld strength.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology d.. |
|||
Melting Point | 282 °C | 540 °F | |
Toyobo TS401 PPS, 40% Glass Fiber Reinforced Key Feature: General Purpose Grade - balanced characteristics suitable for a broad range of uses.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a spec.. |
|||
Melting Point | 282 °C | 540 °F | |
Toyobo TS501 PPS, 50% Glass Fiber Reinforced Key Feature: High stiffnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent physical, e.. |
|||
Melting Point | 282 °C | 540 °F | |
Toyobo TS201 HS PPS, Glass Fiber/Mineral Reinforced Key Feature: High stiffness, high toughnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excel.. |
|||
Melting Point | 282 °C | 540 °F | |
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel.. |
|||
Melting Point | 282 °C | 540 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® OCD2100 BK27021 PA46-GF40 40% Glass Reinforced, Heat Stabilized |
|||
Melting Point | 282 °C | 540 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® OCD2300 BLK PA46-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Melting Point | 282 °C | 540 °F | ASTM D2133 |
Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS) TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Melting Point | 282 °C | 540 °F | ASTM D2133 |
Ensinger TECATRON™ PPS Polyphenylene sulfide (PPS) TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Melting Point | 282 °C | 540 °F | ASTM D2133 |
Ensinger TECATRON™ PVX Polyphenylene sulfide (PPS), Bearing Grade TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Melting Point | 282 - 295 °C | 540 - 563 °F | Average value: 295 °C Grade Count:81 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Melting Point | 282 °C | 540 °F | ASTM D2133 |
Ensinger ENSIFIDE® PPS (Polyphenylene Sulfide) - Extruded Products
(discontinued **) ENSIFIDE is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves ENSIFIDE at.. |