Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 264 °C | 507 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ N1001D-U03 Nylon Standard unreinforced extrusion grade. Main Features:Outstanding fuel barrierHeat resistanceExample of applications:Multi-layered fuel tube |
|||
Melting Point | 264 °C | 507 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ N1001D-U83/02 Nylon Standard unreinforced extrusion grade. Main Features:Outstanding fuel barrierHeat resistanceExample of applications:Multi-layered fuel tube |
|||
Melting Point | 264 °C | 507 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ N1006D-H31 Nylon Standard unreinforced extrusion grade. Main Features:Chemical resistanceLong term heat resistanceExample of applications:Tube applications |
|||
Melting Point | 264 °C | 507 °F | ISO 11357 |
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, DRY Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab.. |
|||
Melting Point | 264 °C | 507 °F | ISO 11357 |
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Melting Point | 264 °C | 507 °F | ASTM D3418 |
Samyang Tramid® 210F Polyamide, High Productivity Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210F is a high productivity grade.Applications:ConnectorsCable tiesHarness clipsT.. |
|||
Melting Point | <= 264 °C | <= 507 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil HDPE HD 8660.29 High Density Polyethylene Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Melting Point | <= 264 °C | <= 507 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil HDPE HD P8660.29 High Density Polyethylene Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Melting Point | <= 264 °C | <= 507 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil HDPE HMA 018 High Density Polyethylene Resin Product Description: HMA 018 is an easy flow HDPE grade, characterized by high gloss and dimensional stability. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabili.. |
|||
Melting Point | 264 °C | 507 °F | DAM; ASTM D3418 |
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance.. |
|||
Melting Point | 264 °C | 507 °F | ISO 3146 |
Eurostar Star L PA66 30V D31 PA66, Glass Fiber Filled, Injection Molded Star L PA66 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Melting Point | 264 °C | 507 °F | ISO 11357-3 |
Ascend Performance Materials Vydyne® R533T Nylon 66, Translucent, 33% Glass Filled, Dry as Molded Vydyne® R533T is a translucent 33% glass-reinforced PA66 resin designed specifically for use in power-steeing reservoirs dn other applications where chemical resistance, whiteness and transmittance.. |