Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 260 °C | 500 °F | |
Plastcom SLOVAMID 66 GF 13 TS PA66, 13% glass fibre FeaturesChemically reinforced with 13% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Melting Point | 260 °C | 500 °F | |
Plastcom SLOVAMID 66 GF 40 PA66, 40% glass fibre FeaturesChemically reinforced with 40% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Melting Point | 260 °C | 500 °F | |
Plastcom SLOVAMID 66 HI/1 TS PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |
|||
Melting Point | 260 °C | 500 °F | (Dry) |
Radici Radilon® A RV150 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Melting Point | 260 °C | 500 °F | Peak Melting Temperature; ASTM D789 |
PolyOne Nymax™ ND 1233 GF Black Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Melting Point | 260 °C | 500 °F | 10°C/min (DAM); ISO 11357-1/-3 |
DSM Akulon® S223-E Nylon 66 (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
DSM Akulon® S224-KMV7 Nylon 66-35% Mineral Reinforced (European and Asian Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Melting Point | 260 °C | 500 °F | ASTM and ISO test |
BASF Capron® 5233G 33% Glass-Filled Nylon 66 (Dry)
(discontinued **) Capron 5233G is a 33% glass fiber reinforced, polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This balance of engineerin.. |
|||
Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance |
|||
Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Durethan® AKV 35 CX H2.0 900876 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Melting Point | 260 - 265 °C | 500 - 509 °F | |
Tisan TISLAMID® 66 15% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melting Point | 260 °C | 500 °F | ISO 3146 |
Wellman Wellamid® FR22F-NBK3 Flame Retardant Nylon 66 Description: Flame Retardant Nylon 66Information provided by Wellman. |
|||
Melting Point | 260 °C | 500 °F | ISO 3146 |
Wellman Wellamid® GS40-66 22L-Bk1 40% Glass Sphere Filled Nylon 66 Description: Glass Sphere Filled Nylon 66Information provided by Wellman. |
|||
Melting Point | 260 °C | 500 °F | ISO 3146 |
Wellman Wellamid® MRGF1647-BK1 Nylon 66, 40% Mineral/Glass Fiber Reinforced All information provided by Wellman Engineered Resins. |
|||
Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
DSM Akulon® S227-C Nylon 66 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® AG-25 HM PA66-GF25 Product description: Grilon AG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA66 injection molding grade with 25% glass fibers. Grilon AG-25 HM has the following important pro.. |
|||
Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® AZ 3/2 PA66 Product description: Grilon AZ 3/2 is an unreinforced and impact modified PA66 injection molding grade. Grilon AZ 3/2 has the following important properties: Excellent toughness at low temperaturesE.. |
|||
Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® GV-2H PA*-GF20 Product description: Grivory GV-2H natural is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide... |
|||
Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® GVS-5H nat PA*-GF50 Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide.. |
|||
Melting Point | 260 °C | 500 °F | ASTM D2133 |
E-Polymers TEKAMID® TA250G60 60% Glass Fiber Reinforced, High Modulus PA66 Resin Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,.. |
|||
Melting Point | 260 °C | 500 °F | ISO 3146/C2 |
Addiplast Addinyl A2 V40 Nylon 66, 40% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Melting Point | 260 °C | 500 °F | ISO 11357-3 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Melting Point | 260 °C | 500 °F | ISO 3146 |
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Dry) Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS .. |
|||
Melting Point | 260 °C | 500 °F | 10 K/min |
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Conditioned) Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Melting Point | 260 °C | 500 °F | DIN 53765 |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Melting Point | 260 °C | 500 °F | ASTM Test |
BASF Ultramid® A3EG7 BK23189 35% Glass Filled PA66 (Dry) Ultramid A3EG6 BK23189 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Melting Point | 260 °C | 500 °F | ASTM D3417 |
Quantum Nylon 6/6 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Melting Point | 260 °C | 500 °F | ISO 11357-3 |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Melting Point | 260 °C | 500 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® FR50 BK505 Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 BK505 is a 25% glass fiber reinforced flame retardant black polyamide 66 resin for injection molding.Information provided by DuPont Perfo.. |