Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 248 - 250 °C | 478 - 482 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET B-105C PET Bottle Grade A co-polymer used for soft drinks and other applications. |
|||
Melting Point | 248 - 260 °C | 478 - 500 °F | Average value: 252 °C Grade Count:5 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep.. |
|||
Melting Point | 248 °C | 478 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman Aqua 20837 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer 20.. |
|||
Melting Point | 248 °C | 478 °F | |
Eastman Eastapak 9921W PET
(discontinued **) Unreinforced. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003. |
|||
Melting Point | 248 - 250 °C | 478 - 482 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET B-07C PET Bottle Grade A co-polymer used mostly for containers. |
|||
Melting Point | 248 - 250 °C | 478 - 482 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET B-101C PET Sheet Grade A sheet grade polymer used in thick films. |
|||
Melting Point | 248 - 250 °C | 478 - 482 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET B-103C PET Bottle Grade A co-polymer used for mineral water bottles |
|||
Melting Point | <= 248 °C | <= 478 °F | DSC |
Indorama Auriga Polymers Polyclear™ Splash 3301 PET Resin Description: Polyclear® Splash PET 3301 is a copolymer packaging resin with a nominal intrinsic viscosity of 0.74 dl/g. Polyclear® Splash PET 3301 is designed to provide very low regenerated a.. |
|||
Melting Point | <= 248 °C | <= 478 °F | M2E-73-002 |
Indorama Ventures Mexico Polyclear™ Splash 3301 PET Resin Description: La resina Polyclear® Splash PET 3301 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.74 dl/g. La resina Polyclear® Splash PET 3301 ha sido .. |
|||
Melting Point | <= 248 °C | <= 478 °F | DSC |
Indorama Auriga Polymers Invistaâ„¢ Polyclearâ„¢ Crystalâ„¢ 3302 PET Resin Description: Polyclearâ„¢ Crystalâ„¢ PET 3302 is a copolymer packaging resin with a nominal intrinsic viscosity of 0.79 dl/g. Polyclearâ„¢ Crystalâ„¢ PET 3302 is designed to have slow re.. |
|||
Melting Point | 248 °C | 478 °F | |
Techmer ES HiFill® PET GF15 X BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Melting Point | <= 248 °C | <= 478 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1001XV Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1001 XV is a C4 Ziegler Natta LLDPE for power cable and Telecom jacketing. The grade contains a low level of antioxidants and has excellent Environmental Stress Crack Resista.. |
|||
Melting Point | <= 248 °C | <= 478 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1002YB Cast Linear Low Density Polyethylene Resin Product Description: LL 1002YB is an LLDPE resin designed for cast films. It offers high gloss and excellent drawdown in both blown and cast film applications. LL 1002YB may also be used as a blend .. |
|||
Melting Point | <= 248 °C | <= 478 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1002YB Wire & Cable Linear Low Density Polyethylene Resin Product Description: LL 1002YB is a C4 Ziegler Natta LLDPE for Low Voltage power cable and Telecom jacketing. The grade contains a higher level of antioxidants and has excellent Environmental Stress.. |
|||
Melting Point | 248 °C | 478 °F | Internal Measurement |
Bapolene® 82 Polyethylene Terephthalate Applications: Water bottles, household, liquor and food containers. All data is based on molded plaques. |