Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 221 °C | 430 °F | Masterbatch; ISO 11357-1,-3 |
Nanocyl PLASTICYL™ PA1503 Polyamide 6 with 1 wt% of Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 F Raw extruded nylon 6 for injection molding Raw extruded nylon 6 for injection molding, highly crystallized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 SG-GV20 Nylon 6 for injection molding, 20% glass fiber reinforced Nylon 6 for injection molding, light impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 UF Nylon 6 for injection molding Nylon 6 for injection molding, highly crystallized, UV stabilizedInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 W-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 D-S10 Nylon 6., std. viscosity for injection molding Nylon 6., std. viscosity for injection molding, permanently flexible, increased dry impact resistance (for dowels).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 EO Raw extruded nylon 6 for injection molding Raw extruded nylon 6 for injection molding, lubricated in surface.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 HS-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 HS-KV30 Nylon 6 for injection molding, 30% glass ball reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 L-HS-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, improved fluidity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 ND Nylon 6 Nylon 6, low viscosity, permanently flexible, dry impact resistant (dowels).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 W-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit FRIANYL B63 W-KV30 Nylon 6 for injection molding, 30% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
Nilit RECONYL B F Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding, highly crystallized (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 221 °C | 430 °F | 10 °C/min; ISO 11357-1,-3 |
Lanxess Durethan® BC 30 S 000000 Nylon 6 PA 6, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
Melting Point | 221 - 225 °C | 430 - 437 °F | |
Johnson Matthey Plumbsol Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Melting Point | 221 - 280 °C | 430 - 536 °F | |
Lucas-Milhaupt Clean & Bright 6 Tin/ Silver Solder Characteristics:This alloy is considered to be high strength solders. It has much higher creep strengths than the tin/lead solders. It is a good color match for stainless steel, and used with the p.. |
|||
Melting Point | 221 °C | 430 °F | |
Heatbath/Park Partherm 430 Heat Transfer Salt A popular heat transfer salt for use in the higher temperature ranges. It is more inert to ferrous alloys than Partherm 290 or 350 and considerably lower in cost. Its heat capacity and thermal cond.. |
|||
Melting Point | 221 - 226 °C | 430 - 439 °F | |
Indium Corp. Indalloy 123 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 221 °C | 430 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® TP 036-052 000000 Nylon 6, 60% Glass Fiber PA 6, injection molding grade, 60% glass fibers, good flowability (Easy Flow), good heat-resistance |
|||
Melting Point | 221 °C | 430 °F | |
Heatbath/Park Tempering C-ALHT for Aluminum Solution Heat Treating A granular mixture of sodium and potassium nitrates formulated per MIL-S-10699-B, class 11 and MIL-H-6088. The salt is colored pink for identification purposesInformation provided by Heatbath Corpo.. |
|||
Melting Point | 221 °C | 430 °F | ISO 11357-1/-3 |
Covestro Makroblend® KU 2-7609 Polycarbonate + PBT, Mineral Filled Impact Grade ISO 7792-1-PC/PBT,MHPR,-030,MD20(PC+PBT)-blendsimpact modifiedInjection molding grade20% mineral filledPreprocessingMax. Water content |
|||
Melting Point | <= 221 °C | <= 430 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 358BW Low Density Polyethylene Resin (European Grade) Product Description: LD 358BW is an EVA LDPE which offers a combination of excellent sealability and toughness even at low temperatures.Availability: Europe Additive: Antiblock: NoSlip: No Thermal .. |
|||
Melting Point | 221 °C | 430 °F | |
Domo Domamid® 32 Polyamide 6 DOMAMID® 32 are Polyamide 6 pellets with a higher viscosity produced from Caprolactam by polymerization.Applications: Standard quality for production of monofilaments and fishing netsInformation pr.. |
|||
Melting Point | 221 °C | 430 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® FN727 BK230A Nylon 6 Zytel® FN727 BK230A is a black, impact modified, plasticizer free, very flexible polyamide 6 alloy resin having good low temperature toughness, good heat aging and good chemical resistance. Uses in.. |
|||
Melting Point | 221 °C | 430 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® FN727 NC010A Nylon 6
(Unverified Data**) Toughened Polyamide 6Information provided by DuPont Performance Polymers |
|||
Melting Point | 221 °C | 430 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF10 MX6 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T.. |
|||
Melting Point | 221 °C | 430 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Melting Point | 221 °C | 430 °F | ASTM D3418 |
Ashley Polymers Ashlene® 149WO PBT Polyester, 45% Glass Reinforced A flame retardant PBT polyester with 45% glass reinforcement, mineral filled.Data provided by the manufacturer |