Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 196 °C | 385 °F | ISO METHOD 3146C |
NYCOA 2046 Copolymer Nylon 6/69 extrusion, moderate melt viscosity, high strength mono.Information provided by NYCOA, Inc. |
|||
Melting Point | 196 - 200 °C | 385 - 392 °F | Average value: 197 °C Grade Count:5 |
Overview of materials for Nylon 6/69 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6/69". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Melting Point | 196 - 204 °C | 385 - 400 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® Clear 15N80 Thermoplastic Polyurethane Elastomer PEARLTHANE® CLEAR 15N80 is a polyether copolymer-based TPU, supplied in form of translucent, colorless, combining low hardness with excellent mechanical properties and excellent hydrolysis resist.. |
|||
Melting Point | 196 °C | 385 °F | ISO 3146 |
Chengdu Polyster H605B Thermoplastic Polyether-ester Elastomer (TPEE) Medium modulus molding and extrusion grade. Contains color-stable antioxidants. Good balance of low and high temperature properties. Good melt stability. CVJ boots, dust cover, bellows, jackets and .. |
|||
Melting Point | 196 °C | 385 °F | Freezing Point; ASTM D3418 |
DuPont™ Bynel® 41E766 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Melting Point | 196 °C | 385 °F | ASTM D3418 |
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET
(Unverified Data**) Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon.. |
|||
Melting Point | 196 °C | 385 °F | ASTM D3418 |
Ashley Polymers Ashlene® 745 Nylon 6/69 A special copolymer ideal for blown and cast film coextrusion. This is a gel free resin with outstanding lot to lot consistency being produced by a continuous process. It has a lower melting point.. |
|||
Melting Point | 196 °C | 385 °F | 10 K/min |
BASF Ultramid® C33 01 PA66/6 (Conditioned) Ultramid C33 01 is an intermediate viscosity PA6/66 grade. Its lower melting point than standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It conforms to F.. |
|||
Melting Point | 196 °C | 385 °F | ASTM Test |
BASF Ultramid® C33 01 PA66/6 (Conditioned) Ultramid C33 01 is an intermediate viscosity PA6/66 grade. Its lower melting point than standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It conforms to F.. |
|||
Melting Point | 196 °C | 385 °F | 10 K/min |
BASF Ultramid® C33L 01 PA66/6 (Dry) Ultramid C33L 01 is an intermediate viscosity, copolymer 6/66.Its lower melting point than standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It conforms to.. |
|||
Melting Point | 196 °C | 385 °F | ASTM D3418 |
Ashley Polymers Ashlene® 746 Nylon 6/69 A special copolymer ideal for blown and cast film coextrusion. This is a gel free resin with outstanding lot to lot consistency being produced by a continuous process. It has a lower melting point.. |
|||
Melting Point | 196 °C | 385 °F | ASTM D3418 |
Ashley Polymers Ashlene® 747 Nylon 6/66 A medium viscosity copolymer. Excellent flexibility and elongation suitable for film and monofilament applications.Data provided by the manufacturer |
|||
Melting Point | 196 °C | 385 °F | 10 K/min |
BASF Ultramid® C33 01 PA66/6 (Dry) Ultramid C33 01 is an intermediate viscosity PA6/66 grade. Its lower melting point than standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It conforms to F.. |
|||
Melting Point | 196 °C | 385 °F | ASTM Test |
BASF Ultramid® C33 01 PA66/6 (Dry) Ultramid C33 01 is an intermediate viscosity PA6/66 grade. Its lower melting point than standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It conforms to F.. |