Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1913 °C | 3475 °F | |
American Elements Indium Oxide Nanopowder General DescriptionIndium Oxide Nanopowder or Nanoparticles (InO), nanodots or nanocrystals are white high surface area particles. Nanoscale Indium Oxide Nanoparticles are typically 5 - 100 nanomete.. |